How to deal with the oxidized white spots of Stainless Steel Capillary Tubings?
Experienced technicians know that white spots are easily formed on the surface of stainless steel pipe fittings after being oxidized. At this time, corresponding treatments must be made, but what should we do?
1. Surface polishing method.
Polishing can fill the pores of stainless steel pipes with the ground aluminum powder.
2. High voltage and high current density impulse method.
In the early stage of anodizing, high-voltage and high-current impacts are adopted, so that the large and small stainless steel pipes that were previously cut by impurities will be connected into pieces after large current impacts.
3. Exterior shot peening method.
Because the power of shot blasting will be greatly improved, the performance of such stainless steel pipe fittings after anodizing and dyeing will be surprisingly good