310S

Chemical Composition

C :≤0.08,
Si :≤1.500,
Mn :≤2.00,
P :≤0.035,
S :≤0.030,
Ni :≤19.00-22.00,
Cr :≤24.00-26.00

Physical Properties:

Strength of extensition (бb)(Mpa) :≥520
Yield Strength (σs)(Mpa) :≥205
Reduction of Area (ψ)% :≥50

Mechanical Property:

ób(MPa)≥520,ó0.2(MPa)≥205 ,δ5(%)≥40, Ψ(%)≥50,HB≤187  Resist  above 1150℃ High temperature。Melting point: 1398℃~1454℃